AME-ST2722 has the characteristics of simple and efficient operation, high measurement accuracy, good stability, good repeatability, and multi-purpose convenient use.
Basic parameters
Specification model | AME-ST2722 |
Resistivity measurement range | 10.0*10-6 to k*200.0*103Ω-cm, k=1 to 10 |
resolution | 1.0*10-6 to 0.1*103Ω-cm, k=1 to 10 |
Range | 10mV to 100 mV, automatic |
DC | 0.1µA, 1.0µA, 10µA, 100µA, 1.0mA, 10mA, 100mA, 1.0A total of 8 levels adjustable |
Some parameters of powder test bench | |
Sample composition | The composition is not limited, but it must not contain components that have a corrosive effect on the test bench and electrodes. |
Sample particle size | 40 mesh to 60 mesh (standard sieve) is recommended. Generally, other particle sizes are also available |
Volume of cup | Section: S = 1.0cm2 Height: 0~20mm adjustable |
Automatic height test unit | |
measurement error | ±0.02mm |
The four-digit effective display | 00.00~20.00mm |
Resolution | ± 0.02mm |
Automatic pressure test unit | |
Standard pressure | P0 = 4Mpa±0.05Mpa |
Pressure range | 20Mpa, P = 0~20 Mpa adjustable |
Four-digit effective display | 00.00~20.00MPa |
resolution | ± 0.01 MPa |
Working power | 220V(110V)±10%, f=50Hz,Pw<10W |
working environment | |
Temperature | 0 ℃~40 ℃ |
Relative humidity | ≤60% |
Note:There should be no strong electromagnetic field interference in the studio |
Reference standard:
Four-probe method
GBT 30835-2014 “Carbon composite lithium iron phosphate anode material for lithium ion batteries”
GB / T 1552-1995 “Four-Probe Method for Measuring Resistivity of Silicon and Germanium Single Crystal”
Four-terminal method
GB / T 24521-2009
YS / T 587.6-2006